Specific Process Knowledge/Etch/ICP Metal Etcher: Difference between revisions
Appearance
| Line 2: | Line 2: | ||
*[[Specific Process Knowledge/Etch/ICP Metal Etcher/nanoetch/180nmzep|The 180 nm zep resist profiles]] | *[[Specific Process Knowledge/Etch/ICP Metal Etcher/nanoetch/180nmzep|The 180 nm zep resist profiles]] | ||
*[[Specific Process Knowledge/Etch/ICP Metal Etcher/nanoetch/340nmzep|The 340 nm zep resist profiles]] | |||
{| border="2" cellspacing="1" cellpadding="3" align="center" | {| border="2" cellspacing="1" cellpadding="3" align="center" | ||
Revision as of 11:51, 18 March 2011
Etching of nanostructures in silicon using the ICP Metal Etcher or DRIE Pegasus
| Sinano3.0 | Sinano3.1 | Sinano3.2 | Sinano3.3 | Sinano3.4 | Sinano4.0 | Sinano3.5 | Sinano3.6 | |
|---|---|---|---|---|---|---|---|---|
| Tool | ICP Metal | ICP Metal | ICP Metal | ICP Metal | ICP Metal | ICP Metal | ICP Metal | ICP Metal |
| Cl2 (sccm) | 0 | 0 | 0 | 0 | 0 | 20 | 15 | 15 |
| BCl3 (sccm) | 5 | 3 | 5 | 5 | 5 | 0 | 5 | 5 |
| HBr (sccm) | 15 | 17 | 15 | 15 | 15 | 0 | 0 | 0 |
| Coil power (W) | 900 (Load) | 900 (Forward) | 900 (Forward) | 900 (Forward) | 900 (Forward) | 900 (Load) | 900 (Load) | 900 (Forward) |
| Platen power (W) | 50 | 50 | 60 | 75 | 90 | 60 | 60 | 60 |
| Pressure (mtorr) | 2 | 2 | 2 | 2 | 2 | 2 | 5 | 10 |
| Process time (s) | 150 | 180 | 120 | 180 | 120 | 90 | 120 | 180 |
| Nominal line width | Etched depths (nm) | |||||||
| 30 nm | 198 | 231 | 147 | 214 | 163 | 227 | 185 | 170 |
| 60 nm | 256 | 308 | 181 | 305 | 229 | 253 | 191 | 185 |
| 90 nm | 259 | 335 | 195 | 342 | 255 | 251 | 222 | 253 |
| 120 nm | 277 | 346 | 203 | 357 | 262 | 257 | 221 | 278 |
| 150 nm | 269 | 341 | 205 | 369 | 265 | 262 | 225 | 280 |
| Nominal line width | Etch rates in trenches (nm/min) | |||||||
| 30 nm | 79 | 77 | 74 | 71 | 82 | 151 | 93 | 57 |
| 60 nm | 102 | 103 | 91 | 102 | 115 | 169 | 96 | 62 |
| 90 nm | 104 | 112 | 98 | 114 | 128 | 167 | 111 | 84 |
| 120 nm | 111 | 115 | 102 | 119 | 131 | 171 | 111 | 93 |
| 150 nm | 108 | 114 | 103 | 123 | 133 | 175 | 113 | 93 |
| Etch rates in zep resist (nm/min) | ||||||||
| zep | 18 | 27 | 35 | 39 | 54 | 45 | 38 | 39 |