[[Image:Tool+operator station.jpg|400px|thumb|RTP2 Jipelec: Position in cleanroom A5]]


The machine consists of a reactor chamber, in which different samples can be processed/annealed at temperatures up to 1200 °C.
The machine consists of a reactor chamber, in which different samples can be processed/annealed at temperatures up to 1200 °C.


The chamber can be heated up very rapidly by the use of 18 infrared halogen lamps that are situated in the chamber lid. A quartz plate is placed below the lamps, i.e. between the lamps and the sample(s). Below the platen, there is an optical pyrometer aligned with the center of the substrate, that is placed on the bottom part of the chamber. The platen presents additional inlets where multiple thermocouples can be mounted. These details are exemplified in images below.
The chamber can be heated up very rapidly by the use of 18 infrared halogen lamps that are situated in the chamber lid. A quartz plate is placed below the lamps, i.e. between the lamps and the sample(s). Below the platen, there is an optical pyrometer aligned with the center of the substrate, that is placed on the bottom part of the chamber. The platen presents additional inlets where multiple thermocouples can be mounted. These details are exemplified in images below.
[[Image:Jipelec RTP 2.jpg|650x650px|thumb|RTP Jipelec 2: Positioned in cleanroom A-5]]


'''The user manual, user APV, technical information and contact information can be found in LabManager:'''
'''The user manual, user APV, technical information and contact information can be found in LabManager:'''

Revision as of 13:39, 6 November 2023

Feedback to this page: click here

This page is written by DTU Nanolab internal

THIS PAGE IS UNDER CONSTRUCTION

RTP2 Jipelec - Rapid Thermal Processor

The main purpose of the RTP2 Jipelec (Jipelec JetFirst 200 RTP) is to perform thermal processes, using faster heating rates and shorter process durations when compared to conventional methods. This is called rapid thermal processing (RTP) and can be used to treat different types of samples.

Rapid thermal processing typically includes RTA, i.e. Rapid Thermal Annealing, where samples are heated up very rapidly in a nitrogen or argon atmosphere. Contact alloying and RTN, i.e. Rapid Thermal Nitridation, might also be possible for some samples.

The Set-Up

RTP2 Jipelec: Position in cleanroom A5

The machine consists of a reactor chamber, in which different samples can be processed/annealed at temperatures up to 1200 °C.

The chamber can be heated up very rapidly by the use of 18 infrared halogen lamps that are situated in the chamber lid. A quartz plate is placed below the lamps, i.e. between the lamps and the sample(s). Below the platen, there is an optical pyrometer aligned with the center of the substrate, that is placed on the bottom part of the chamber. The platen presents additional inlets where multiple thermocouples can be mounted. These details are exemplified in images below.

The user manual, user APV, technical information and contact information can be found in LabManager:

RTP Jipelec 2

Overview of the performance of the Jipelec RTP and some process related parameters

Purpose Rapid thermal processor/annealer
Process parameter range Process temperature

Annealing temperature:

  • Up to 1200 oC, but maximum 450 oC for III-V materials
    • Time limits at temperatures above 700 oC:
      • 700 °C: 60 min.
      • 800 °C: 30 min.
      • 900 °C: 20 min.
      • 1000 °C: 10 min.
      • 1100 °C: 5 min.
      • 1200 °C: 1 min.

Temperature ramp:

  • Up to 50 oC/min with susceptor
  • Up to 100 oC/min without susceptor
Process pressure
  • 1 atm (atmospheric pressure)
  • ~ 0 mbar (vacuum) without any gas flow
Gases on the system

Process gases:

  • Nitrogen (N2)
  • Argon (Ar)
  • Forming gas (4 % H2/96 % N2) - Not connected yet

Purge gas:

  • Nitrogen (N2)
Substrates Batch size
  • One 200 mm wafer (less good temperature uniformity than smaller wafers/samples)
  • One 150 mm wafer
  • One 100 mm wafer
  • One or more 50 mm wafers (always placed on a susceptor or carrier wafer)
  • One or more small samples (always placed on a susceptor or carrier wafer)
Substrate materials allowed
  • Silicon
  • Silicon oxide and silicon nitride
  • Fused silica/quartz
  • III-V materials - Use a dedicated carrier wafer
  • Metals - Use a dedicated carrier wafer and ask for permission