<gallery caption="SiO2 etch with Cr mask on wafer piece on Si carrier 6 min etch, H2:0sccm, C4F8:13sccm He:225sccm, Pressure:3.35mTorr" perrow="6" widths="200px" heights="150px"> | <gallery caption="SiO2 etch with Cr mask on wafer piece on Si carrier 6 min etch, H2:0sccm, C4F8:13sccm He:225sccm, Pressure:3.35mTorr" perrow="6" widths="200px" heights="150px"> | ||
File:C10082_07.jpg | File:C10082_07.jpg | ||
File: | File:C010082top_07.jpg | ||
File: | File:C010082top_03.jpg | ||
File: | File:C010082tilt30_13.jpg | ||
</gallery> | </gallery> | ||