<gallery caption="SiO2 etch with Cr mask on wafer piece on Si carrier 6 min etch, H2:0sccm, C4F8:13sccm He:215sccm O2:10sccm, Pressure:3.35mTorr; platen power 150W, coil power:1200W" perrow="6" widths="200px" heights="150px">