*Sample: s007592 ''by bghe@nanolab (2015-06-02)''
*Sample: s007592 ''by bghe@nanolab (2015-06-02)''
*See Martin Lind Ommen's results with hard masks: [https://labadviser.nanolab.dtu.dk//index.php?title=Specific_Process_Knowledge/Etch/Etching_of_Silicon_Oxide] <br> There were problems with polymer on the surface after etching.
*See Martin Lind Ommen's results with hard masks: [https://labadviser.nanolab.dtu.dk//index.php?title=Specific_Process_Knowledge/Etch/Etching_of_Silicon_Oxide#Dry etch with Hard mask] <br> There were problems with polymer on the surface after etching.
|}
|}