Jump to content

Specific Process Knowledge/Back-end processing/Polymer Injection Molder: Difference between revisions

From LabAdviser
Choi (talk | contribs)
No edit summary
Choi (talk | contribs)
mNo edit summary
Line 1: Line 1:
The injection molding machine is located in the basement of building 346 (room 904). It is an Engel Victory 80/45 Tech.
The injection molding machine is located in the basement of building 346 (room 904). It is an Engel Victory 80/45 Tech.
The machine can be booked from LabManager (not active yet).
The machine can be booked from LabManager. The machine is called "Polymer Injection Molding".


[[Image:Imm.jpg|Picture of IMM]]
[[Image:Imm.jpg|Picture of IMM]]
Line 7: Line 7:


'''Polystyrene'''
'''Polystyrene'''
(Total Petrochemicals)
(BASF Polystyrol 158K)


'''Topas (COC from Ticona)'''
'''Topas (COC from Ticona)'''

Revision as of 09:39, 25 May 2011

The injection molding machine is located in the basement of building 346 (room 904). It is an Engel Victory 80/45 Tech. The machine can be booked from LabManager. The machine is called "Polymer Injection Molding".

Picture of IMM

The following polymers are presently available:

Polystyrene (BASF Polystyrol 158K)

Topas (COC from Ticona) 5013S-04 6015S-04 6017S-04 8007S-04

Other polymers (PE, PBT, PCT, PC, POM, PP, PU, SAN) are available in smaller amounts. Ask Danchip for details (choi@danchip.dtu.dk).