Specific Process Knowledge/Etch/DRIE-Pegasus/Isotropic/mediumiso1: Difference between revisions
Appearance
No edit summary |
No edit summary |
||
| Line 3: | Line 3: | ||
<!--Checked for updates on 2/10-2020 - ok/jmli --> | <!--Checked for updates on 2/10-2020 - ok/jmli --> | ||
<!--Checked for updates on 28/6-2023 - ok/jmli --> | <!--Checked for updates on 28/6-2023 - ok/jmli --> | ||
<!--Checked for updates on 4/9-2025 - ok/jmli --> | |||
{{contentbydryetch}} | {{contentbydryetch}} | ||
Latest revision as of 10:40, 4 September 2025
Feedback to this page: click here Unless otherwise stated, the content of this page was created by the dry etch group at DTU Nanolab
| Date | Substrate Information | Process Information | SEM Images | ||||||
|---|---|---|---|---|---|---|---|---|---|
| Wafer info | Mask | Material/ Exposed area | Tool / Operator | Conditioning | Recipe | Wafer ID | Comments | ||
| 9/4-2014 | 4" | travka05 wafer 1.5 µm AZ | Si / 5 % | Pegasus/jmli | 5 minute TDESC clean + MU runs | jml/isotropic/mediumiso1 2:00 minutes | S003961 | ||
| 6/6-2016 | 6" | travka35 wafer 1.5 µm AZ | Si / 35 % | Pegasus/jmli | standard/danchip/mediumiso1 2:00 minutes | S006534 | |||
| 6/6-2016 | 6" | travka35 wafer 1.5 µm AZ | Si / 35 % | Pegasus/jmli | standard/danchip/mediumiso1 4:00 minutes | S006535 | |||