LabAdviser/314/Preparation 314-307/Coating: Difference between revisions
No edit summary |
|||
Line 18: | Line 18: | ||
== Quorum Q150T Sputter Coater and Glow discharge == | == Quorum Q150T Sputter Coater and Glow discharge == | ||
[ | [https://labmanager.dtu.dk/view_binary.php?class=MiscDocument&id=15&name=Q150T_Instruction_Manual_10473_iss3+%281%29.pdf0 Manual] ''- requires login'' | ||
[[File:Quorum coater.jpg|400px|left|thumb|Location Building 314, Prep Room 03]]<br /> | [[File:Quorum coater.jpg|400px|left|thumb|Location Building 314, Prep Room 03]]<br /> | ||
Line 30: | Line 30: | ||
[[File:IMG_3685.JPG|250px|left|thumb|Quorum Q150T Sputter Coater Location Building 314, Prep Room 01]]<br /> | [[File:IMG_3685.JPG|250px|left|thumb|Quorum Q150T Sputter Coater Location Building 314, Prep Room 01]]<br /> | ||
<br clear="all" /> | <br clear="all" /> --> | ||
Accessory for 208HR Sputter Coater | ===Accessory for 208HR Sputter Coater=== | ||
Glow Discharge Head | Glow Discharge Head | ||
Line 39: | Line 39: | ||
[[File:IMG_3687.JPG|250px|left|thumb|Location Building 314, Prep Room 01]]<br /> | [[File:IMG_3687.JPG|250px|left|thumb|Location Building 314, Prep Room 01]]<br /> | ||
<br clear="all" / | <br clear="all" /> |
Revision as of 15:41, 27 June 2023
Feedback to this page: click here
This section is written by DTU Nanolab internal if nothing else is stated.
Coaters & Accessories
Cressington 208 Carbon Coater
Quorum Q150T Sputter Coater and Glow discharge
Manual - requires login
Accessory for 208HR Sputter Coater
Glow Discharge Head