Jump to content

Specific Process Knowledge/Thermal Process/Oxidation/Wet oxidation E1 furnace: Difference between revisions

Paphol (talk | contribs)
No edit summary
Paphol (talk | contribs)
No edit summary
Line 3: Line 3:
<i> Unless otherwise stated, this page is written by <b>DTU Nanolab internal</b></i>
<i> Unless otherwise stated, this page is written by <b>DTU Nanolab internal</b></i>


An acceptance test has been done after the installation in November 2021 by Tempress. For wet oxidation at 1050 C and 30 minutes, the thickness variation over a wafer was 1.3%(wafer in wafer), over the boat was 0.35%(wafer to wafer) and ran to ran was 0.64%.
An acceptance test was done after the installation in November 2021 by Tempress. For wet oxidation at 1050 C and 30 minutes, the thickness variation over a wafer was 1.3%(wafer in wafer), over the boat was 0.35%(wafer to wafer) and ran to ran was 0.64%.




[[File:Wet1050_Acceptance_test.PNG|1100x1100px|center|thumb|Acceptance test by Tempress from November 2021.]]
[[File:Wet1050_Acceptance_test.PNG|1100x1100px|center|thumb|Acceptance test by Tempress from November 2021.]]