Pegasus 2 stands out as it is a dedicated research tool where much fewer processes are allowed. As such, the instrument will not be released for general use for a wide range of applications. | Pegasus 2 stands out as it is a dedicated research tool where much fewer processes are allowed. As such, the instrument will not be released for general use for a wide range of applications. | ||
Whereas Pegasus 1 and 3 are intended to serve as stable platforms with limited or no changes in hardware, Pegasus 2 has been subject to experiments. For instance, as of the end of 2020 the instrument has been set up to run | Whereas Pegasus 1 and 3 are intended to serve as stable platforms with limited or no changes in hardware, Pegasus 2 has been subject to experiments. For instance, as of the end of 2020 the instrument has been set up to run [[Specific_Process_Knowledge/Etch/DRIE-Pegasus/Pegasus-2#Publications_on_the_CORE_process|the CORE process]]. This means that comparing to [[Specific_Process_Knowledge/Etch/DRIE-Pegasus/Pegasus-1|DRIE-Pegasus 1]] and [[Specific_Process_Knowledge/Etch/DRIE-Pegasus/Pegasus-3|DRIE-Pegasus 3]], Pegasus 2 and its allowed usage have been modified (this list is not complete - see the complete list in the table below). For instance: | ||
[[ | |||
# The C<sub>4</sub>F<sub>8</sub> MFC has been disconnected to maintain a carbon-free (carbon containing masks are allowed) chamber. | # The C<sub>4</sub>F<sub>8</sub> MFC has been disconnected to maintain a carbon-free (carbon containing masks are allowed) chamber. | ||
# The RF generator supplying the power to the coil has been disconnected thus allowing only processes driven by the platen generator. | # The RF generator supplying the power to the coil has been disconnected thus allowing only processes driven by the platen generator. | ||