Jump to content

Specific Process Knowledge/Characterization/KLA-Tencor Surfscan 6420: Difference between revisions

From LabAdviser
Pevo (talk | contribs)
No edit summary
Reet (talk | contribs)
Line 3: Line 3:
''This page is written by DTU Nanolab  internal''
''This page is written by DTU Nanolab  internal''


==<span style="color:Red">EXPIRED. The KLA-Tencor Surfscan 6420 has has been removed from the cleanroom in April 2023. It has been replaced with the Particle Scanner Takano that can be used instead.</span>==
==<span style="color:Red">EXPIRED. The KLA-Tencor Surfscan 6420 has has been removed from the cleanroom in April 2023. It has been replaced with the [Specific Process Knowledge/Characterization/Particle Scanner Takano|Particle Scanner Takano] that can be used instead.</span>==


== KLA-Tencor Surfscan 6420 ==
== KLA-Tencor Surfscan 6420 ==

Revision as of 14:57, 13 June 2023

Feedback to this page: click here

This page is written by DTU Nanolab internal

EXPIRED. The KLA-Tencor Surfscan 6420 has has been removed from the cleanroom in April 2023. It has been replaced with the [Specific Process Knowledge/Characterization/Particle Scanner Takano|Particle Scanner Takano] that can be used instead.

KLA-Tencor Surfscan 6420

The KLA-Tencor Surfscan (at the place in California where it was refurbished).

The KLA-Tencor is a surface analysis instrument for detecting, couting and sizing of particles, i.e. light point defects. A broad range of particles size from 0.15 µm to greater than 3 µm can be measured on a polished silicon surface with or without or epitaxial layers. The particle contamination in thin films like nitride, oxide and polymer or resist layers can also be inspected. The system will remove small surface roughness, so it will not count as particle contaminations.

The system is mainly being used for quality control of the PECVDs and LPCVD nitride furnaces in the cleanroom.

Users will have to contact the responsible persons (the Thin Film group), if they want to make some particle measurements.

Surfscan 6420


Process information


Overview of the performance of the Surfscan 6420 and some process related parameters

Purpose
  • Detecting, counting and sizing of particles (light point defects)
Performance Particles size
  • 0.15 µm to > 3 µm
Througput
  • Up to 100 wafer per hour (200 mm)
Repeatbility
  • Within 1%, 1σ (mean count > 500, 0.204 µm diameter latex spheres)
Process parameter range Process Temperature
  • Room temperature
Substrates Batch size
  • 1-25 100 mm wafers
  • 1-25 150 mm wafers
  • 1-25 200 mm wafers (the loader has to be changed)
Substrate materials allowed
  • Silicon
  • Thin layers of oxide, nitride and polymer/resist