Specific Process Knowledge/Wafer Information: Difference between revisions

From LabAdviser
Tg (talk | contribs)
New page: == Wafer Information == DTU Danchip has a stock of most used silicon and glass wafers; most of these wafers are to be found in stock in cleanroom 2. Whenever you take a wafer from stock, y...
 
Tg (talk | contribs)
No edit summary
Line 5: Line 5:


{| border="1" style="text-align: center; width: 550px; height: 100px;"
{| border="1" style="text-align: center; width: 550px; height: 100px;"
|colspan="3" style="text-align: center;" style="background: #efefef;" | '''wafer names'''
|colspan="3" style="text-align: center;" style="background: #efefef;" | '''Origin of waferbox names'''
|-
|-
!scope="row" width="30%"|O
!width="30%"|O
!width="35%" |P
!width="35%" |P
!width="35%" |337
!width="35%" |337
Line 22: Line 22:


{| border="1" style="text-align: center; width: 550px; height: 100px;"
{| border="1" style="text-align: center; width: 550px; height: 100px;"
|colspan="3" style="text-align: center;" style="background: #efefef;" | '''wafer available at DTU Danchip'''
|colspan="6" style="text-align: center;" style="background: #efefef;" | '''wafer available at DTU Danchip'''
|-
|-
!scope="row" width="15%"| 
!scope="row" width="15%"| 
Line 74: Line 74:
=== Wafer boxes and single wafer carriers ===
=== Wafer boxes and single wafer carriers ===


New clean wafer boxes and single wafer carriers can be found in the changing area. Ask DTU Danchip personnel for help if stock is low.
New clean wafer boxes and single wafer carriers can be found in the changing area. Ask DTU Danchip personnel for help if stock is low

Revision as of 11:49, 21 December 2010

Wafer Information

DTU Danchip has a stock of most used silicon and glass wafers; most of these wafers are to be found in stock in cleanroom 2. Whenever you take a wafer from stock, you should fill out the logbook with date, name, company, project/team, waferbox name and price per wafer. The Price can also be found in the logbook.

The waferbox name consists of two characters and three to four numbers, eg OP337, according to the code below:

Origin of waferbox names
O P 337
Indicates the company where the wafers are bought Type of doping in the wafer shipment number


Wafers available at DTU Danchip

wafer available at DTU Danchip
  Shelf Size Type Thickness Resistivity
SSP (single side polished) bottom 4" N+P 525 µm 1-20 Ωcm
SSP (single side polished) top 6" N or P 625 µm 1-20 Ωcm
DSP (double side polished) middle 4" N+P 350 µm 1-20 Ωcm
wafers with different layers top 4" and 6"      
Boron glasswafers middle 4"   1 mm  


Wafer boxes and single wafer carriers

New clean wafer boxes and single wafer carriers can be found in the changing area. Ask DTU Danchip personnel for help if stock is low