The thickest achievable coating using a normal spin cycle is | The thickest achievable coating using a normal spin cycle is 10 µm. However, reducing the spin-off time to a few seconds at 2000 rpm, has successfully been used to increase the coating thickness beyond 20 µm on a Gamma coater. The substrate waits for 1 min before softbake, in order to reduce the edge bead height. | ||