'''Feedback to this page''': '''[mailto:danchipsupport@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Back-end_processing/Wire_Bonder#Ball_Wire_Bonder_K.26S_4524 click here]''' | '''Feedback to this page''': '''[mailto:danchipsupport@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Back-end_processing/Wire_Bonder#Ball_Wire_Bonder_K.26S_4524 click here]''' | ||
<!-- Replace "http://labadviser.danchip.dtu.dk/..." wih the link to the Labadviser page--> | <!-- Replace "http://labadviser.danchip.dtu.dk/..." wih the link to the Labadviser page--> | ||
{{CC1}} | {{CC1}} | ||
Revision as of 15:39, 27 March 2023
Feedback to this page: click here
TPT Wire Bonder

Packlab, Building 347, 1st floor
Will be temporary taken out of service during the PolyFabLab construction.
The TPT Wire Bonder is bought i 2007. Wire bonding is a method of making interconnections between a microchip and other electronics as part of semiconductor device fabrication. The TPT-H05 is a manuel wire bonder. It is possible to do wedge bonding with either aluminum wires or gold wires as well as gold ball bonding.
The user manual(s), user APV(s), technical information and contact information can be found in LabManager:
Ball Wire Bonder K&S 4524

Packlab, Building 347, 1st floor

Will be moved to building 451 during the PolyFabLab construction.
The Ball Wire Bonder K&S 4524 is for high precision ball bonding. It is a semi-automatic wire bonder with good control of bond placement and bonding parameters.
The user manual(s), quality control procedure(s) and results, user APV(s), technical information and contact information can be found in LabManager:
| Equipment | TPT Wire Bonder | Ball Wire Bonder | |
|---|---|---|---|
| Purpose |
|
| |
| Performance |
|
| |
| Substrates | Allowed materials |
| |