Specific Process Knowledge/Etch/DRIE-Pegasus/Pegasus-2/ORE with Al2O3 mask: Difference between revisions
Appearance
| Line 133: | Line 133: | ||
| '''R-step''' || 10 || 100% || 0 || 40 || 40 | | '''R-step''' || 10 || 100% || 0 || 40 || 40 | ||
|- | |- | ||
| '''E<sub>1</sub>-step''' || 2 || 220 mTorr || 0 || 350 || | | '''E<sub>1</sub>-step''' || 2 || 220 mTorr || 0 || 350 || 0 | ||
|- | |- | ||
| '''E<sub>2</sub>-step''' || * || 220 mTorr || 0 || 350 || 300 | | '''E<sub>2</sub>-step''' || * || 220 mTorr || 0 || 350 || 100-300 | ||
|} ''*The E<sub>2</sub>-time value was changed and observed.'' | |} ''*The E<sub>2</sub>-time value was changed and observed.'' | ||
<br clear="all" /> | <br clear="all" /> | ||