Jump to content

Specific Process Knowledge/Characterization/Thickness Measurer: Difference between revisions

From LabAdviser
Rkch (talk | contribs)
No edit summary
Mmat (talk | contribs)
mNo edit summary
Line 1: Line 1:
'''Unless anything else is stated, everything on this page, text and pictures are made by DTU Nanolab.'''
{cc-nanolab}}
 
'''All links to Kemibrug (SDS) and Labmanager Including APV and QC requires login.'''


'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Characterization/Thickness_Measurer click here]'''  
'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Characterization/Thickness_Measurer click here]'''  
 
<br>
<br>
==Thickness measurer==
==Thickness measurer==
[[Image:Thicknessmeasurer2007.jpg|thumb|300x300px|Thickness Measurer. Positioned in cleanroom D-3]]
[[Image:Thicknessmeasurer2007.jpg|thumb|300x300px|Thickness Measurer. Positioned in cleanroom D-3]]

Revision as of 16:13, 2 June 2025

{cc-nanolab}}

Feedback to this page: click here

Thickness measurer

Thickness Measurer. Positioned in cleanroom D-3

There are 2 thickness measurers in the cleanroom, both positioned in cleanroom D-3. The Thickness measurer is for measuring all sorts of samples. The thickness measurer (wafers) is solely for measuring the thickness of wafers or depths of grooves on wafers.

During a KOH etch it can be helpful to ensure no over-etching by making a thickness measurement during the etching.


The user manual, technical information and contact information can be found in LabManager:

Thickness measurer Thickness measurer (wafers)

Quality Control - Recipe Parameters and Limits

Quality Control (QC) for the Thickness measurer

The measured standard thickness is 0.1 mm. The measured result has to be within ± 0.005 mm. The QC is preformed once a year.

Equipment performance and process related parameters

Purpose

Thickness measurer

  • Wafer thickness
  • Depths of larger grooves
  • Heigth of larger samples

Performance

Thickness resolution

  • < 1 µm

Substrates

Batch size

  • One sample
Substrate materials allowed
  • No restrictions



Purpose

Thickness measurer (wafers)

  • Wafer thickness
  • Depths of larger grooves

Performance

Thickness resolution

  • < 1 µm

Substrates

Batch size

  • One sample
Substrate materials allowed
  • Only wafers