=Probe Station= | |||
[[Image:probe2.jpg|thumb|300x300px|Probe station. Positioned in serviceroom CX1]] | [[Image:probe2.jpg|thumb|300x300px|Probe station. Positioned in serviceroom CX1]] | ||
The Probe station is a - EPS150Triax - Cascade. The purpose is to measure I/V measurement, ohmic measurements etc. It has 4 individually adjustable triax connected probes, but can be fitted with additional coax connected probes. The stage can be moved in x and y to step and repeat a measurement over a large number of chips. | The Probe station is a - EPS150Triax - Cascade. The purpose is to measure I/V measurement, ohmic measurements etc. It has 4 individually adjustable triax connected probes, but can be fitted with additional coax connected probes. The stage can be moved in x and y to step and repeat a measurement over a large number of chips. | ||
Revision as of 19:45, 27 May 2025
The content on this page, including all images and pictures, was created by DTU Nanolab staff, unless otherwise stated.
Feedback to this page: click here
Probe Station

The Probe station is a - EPS150Triax - Cascade. The purpose is to measure I/V measurement, ohmic measurements etc. It has 4 individually adjustable triax connected probes, but can be fitted with additional coax connected probes. The stage can be moved in x and y to step and repeat a measurement over a large number of chips.
Samples can be inspected by either a microscope and/or a camera.
Two Keithley 2450 source meters are connected to the probe station by triax cables. An additional Keithley 2410 source meter and a Keithley 2000 multi meter is connected by coax cables. All Keithleys can also be connected with banana wires.
|
Purpose |
Electrical measurements |
|
|---|---|---|
|
Performance |
Pad size |
|
|
Substrates |
Batch size |
|
| Substrate materials allowed |
|
The user manual, technical information and contact information can be found in LabManager: