Jump to content

Specific Process Knowledge/Thermal Process/RTP Annealsys: Difference between revisions

From LabAdviser
Indiogo (talk | contribs)
Tag: Manual revert
Indiogo (talk | contribs)
Line 7: Line 7:
''January 2023: The RTP Annealsys is being tested, but it is not released for general use yet. Please contact thinfilm@nanolab.dtu.dk for more information.''
''January 2023: The RTP Annealsys is being tested, but it is not released for general use yet. Please contact thinfilm@nanolab.dtu.dk for more information.''


'''RTP Annealsys (RTP AS-Premium, serial number AS0415C4 - 7484, from ANNEALSYS)''' is a research tool available at DTU Nanolab that can reach very high temperatures in a matter of a few minutes or even seconds. Therefore, it is able to perform several types of rapid thermal processing and it can be used as a multi-functional and versatile microfabrication tool, within specific process windows for each process type, using Si/nanofabricated Si structures. Amongst them, there is rapid thermal annealing '''(RTA)''', hydrogenation '''(RTH)''', oxidation '''(RTO)''', nitridation '''(RTN)''', etc. Currently, it is used for '''rapid thermal annealing and smoothing''' of silicon-based samples.
'''RTP Annealsys (RTP AS-Premium, serial number AS0415C4 - 8177, from ANNEALSYS)''' is a research tool available at DTU Nanolab that can reach very high temperatures in a matter of a few minutes or even seconds. Therefore, it is able to perform several types of rapid thermal processing and it can be used as a multi-functional and versatile microfabrication tool, within specific process windows for each process type, using Si/nanofabricated Si structures. Amongst them, there is rapid thermal annealing '''(RTA)''', hydrogenation '''(RTH)''', oxidation '''(RTO)''', nitridation '''(RTN)''', etc. Currently, it is used for '''rapid thermal annealing and smoothing''' of silicon-based samples.


[[File:LL&station Annealsys.png|450px|thumb|right|The RTP Annealsys work station and loadlock are located in the DTU Nanolab cleanroom B-1. Photo: Maria Farinha@DTU Nanolab, February 2023]]
[[File:LL&station Annealsys.png|450px|thumb|right|The RTP Annealsys work station and loadlock are located in the DTU Nanolab cleanroom B-1. Photo: Maria Farinha@DTU Nanolab, February 2023]]
Line 15: Line 15:
The RTP Annealsys system is divided into two main parts: the process chamber and the loadlock.
The RTP Annealsys system is divided into two main parts: the process chamber and the loadlock.


The chamber has stainless steel walls (water-cooled) and a top and bottom halogen lamp-configuration (32 infra-red lamps, in total). As such, the samples are rapidly heated from both sides, simultaneously. In addition, the chamber is enclosed by two quartz-windows (immediately below/above the set of top/bottom lamps) and these are air-cooled. It is also connected to two external vacuum pumps, to a gas inlet and the loadlock. Similarly, the loadlock is connected to two external pumps.
The chamber has stainless steel walls (water-cooled) and a top and bottom halogen lamp-configuration (28 infra-red lamps, in total). As such, the samples are rapidly heated from both sides, simultaneously. In addition, the chamber is enclosed by two quartz-windows (immediately below/above the set of top/bottom lamps) and these are air-cooled. It is also connected to two external vacuum pumps, to a gas inlet and the loadlock. Similarly, the loadlock is connected to two external pumps.


Moreover, the chamber and the loadlock are separated by the gate valve. While processing, the valve remains closed; it is only opened to exchange the substrates when both chamber and loadlock are under turbo vacuum. The substrate transfer is possible due to the mechanical, retractable arm.
Moreover, the chamber and the loadlock are separated by the gate valve. While processing, the valve remains closed; it is only opened to exchange the substrates when both chamber and loadlock are under turbo vacuum. The substrate transfer is possible due to the mechanical, retractable arm.

Revision as of 10:45, 9 February 2023

THIS PAGE IS UNDER CONSTRUCTION

RTP Annealsys - Rapid Thermal Processor

This page is written by Inês Diogo@DTU Nanolab if nothing else is stated.

January 2023: The RTP Annealsys is being tested, but it is not released for general use yet. Please contact thinfilm@nanolab.dtu.dk for more information.

RTP Annealsys (RTP AS-Premium, serial number AS0415C4 - 8177, from ANNEALSYS) is a research tool available at DTU Nanolab that can reach very high temperatures in a matter of a few minutes or even seconds. Therefore, it is able to perform several types of rapid thermal processing and it can be used as a multi-functional and versatile microfabrication tool, within specific process windows for each process type, using Si/nanofabricated Si structures. Amongst them, there is rapid thermal annealing (RTA), hydrogenation (RTH), oxidation (RTO), nitridation (RTN), etc. Currently, it is used for rapid thermal annealing and smoothing of silicon-based samples.

The RTP Annealsys work station and loadlock are located in the DTU Nanolab cleanroom B-1. Photo: Maria Farinha@DTU Nanolab, February 2023

The Set-Up

The RTP Annealsys system is divided into two main parts: the process chamber and the loadlock.

The chamber has stainless steel walls (water-cooled) and a top and bottom halogen lamp-configuration (28 infra-red lamps, in total). As such, the samples are rapidly heated from both sides, simultaneously. In addition, the chamber is enclosed by two quartz-windows (immediately below/above the set of top/bottom lamps) and these are air-cooled. It is also connected to two external vacuum pumps, to a gas inlet and the loadlock. Similarly, the loadlock is connected to two external pumps.

Moreover, the chamber and the loadlock are separated by the gate valve. While processing, the valve remains closed; it is only opened to exchange the substrates when both chamber and loadlock are under turbo vacuum. The substrate transfer is possible due to the mechanical, retractable arm.

Schematic representation of the rapid thermal processor set-up profile view. The substrate (in green) rests on top of three quartz pins, supported by a quartz holder (in black). The drawing is not to scale. Image: Inês Diogo@DTU Nanolab, December 2022

Temperature Measurement and Control

RTP Annealsys offers an optical pyrometry system for temperature measurement, not requiring any contact with the wafer.

Regarding setting the process temperature, it is also important to mention the tool can function under two distinct modes – power and temperature/pyro control modes. In other words, using power control mode, the tool is programmed to fix the lamp’s power at a specific value (%) and consequently, the temperature inside the chamber varies with time; using the temperature/pyro control mode, the tool is programmed to vary the lamps’ power to maintain the temperature stable and constant inside the chamber at a previously established value in the recipe.

Samples and Process Specifications

The RTP Annealsys, with a base pressure of 10-6 mbar, is a research tool. As such, there are some parameters and details to consider.

Specifics Range Comments
Temperature Temperature Control
  • up to 1200 oC
The maximum temperature allowed is dependent on both processing type and time.
Power Control
  • 0% - 100%
Process gas Ar
  • up to 2000 SCCM
O2
  • up to 2000 SCCM
Not allowed for users.
NH3
  • up to 2000 SCCM
Not allowed for users.
5% H2/Ar
  • up to 2000 SCCM
Pressure Valve (APC)
  • 0o - 90o
Controller
  • up to 12 mbar
Process time
  • 0.1s to 2h46min
Heating rate
  • Max. 150 oC/s
Substrates Batch size
  • Single-wafer process
Substrate size
  • Chips on carrier
  • 100 mm or 150 mm wafers
Small samples must be placed on dedicated carrier wafers. These do not need to be bonded to the carriers.
Allowed materials
  • Silicon
  • Silicon Nitride
  • Aluminum Oxide
Silicon nitride and aluminum oxide are only used as coating/masking materials and have been proven capable of sustaining this type of high temperature processing.

Previous work on RTP Annealsys

More information and details about each type of processing - achievable using the RTP Annealsys tool - can be found in the following documents.

Important! The RTO sequences that were developed during the previous experimental work on the RTP Annealsys are not available to users. More tests and further investigation are required to prevent damaging the tool.

Feedback to this page: click here