Jump to content

Specific Process Knowledge/Bonding/Fusion bonding: Difference between revisions

From LabAdviser
Sifkle (talk | contribs)
No edit summary
Mmat (talk | contribs)
mNo edit summary
 
Line 1: Line 1:
{{cc-nanolab}}
'''Feedback to this page''': '''[mailto:photolith@Nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Bonding/Fusion_bonding click here]'''
'''Feedback to this page''': '''[mailto:photolith@Nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Bonding/Fusion_bonding click here]'''
 
<br>
'''Unless anything else is stated, everything on this page, text and pictures are made by DTU Nanolab.'''
<br>
 
==Fusion Bonding==
==Fusion Bonding==



Latest revision as of 19:13, 27 May 2025

The content on this page, including all images and pictures, was created by DTU Nanolab staff, unless otherwise stated.

Feedback to this page: click here

Fusion Bonding

Fusion bonding is a relative weak bond between e.g. two clean Si wafers. It is absolutely necessary for the wafers to be very clean and to be annealed at 1000°C afterwards to avoid and minimize defects. Fusion bonding can be made as a Si to Si direct bonding or with SiO2 layers in between. It is also possible to use nitride in between but it should be close to 100% particle free. We have good experience with Sintef but unfortunately not with the old DTU Nanolab nitride furnace.

Try and put a fusion bonding as early in a process sequence as possible, since during annealing is not possible to have any kind of metals on your wafer. Furthermore the thermal budget could drive dopants further into the wafer than wanted.