Specific Process Knowledge/Etch/DRIE-Pegasus/Pegasus-4/Barc Etch: Difference between revisions
Appearance
No edit summary |
|||
| Line 1: | Line 1: | ||
==Barc etch with O2== | ==Barc etch with O2== | ||
{{CC-bghe2}}''June 2020'' | {{CC-bghe2}}, ''June 2020'' | ||
===Sample=== | ===Sample=== | ||
*6" Si | *6" Si | ||