==Developer: TMAH Stepper==
==Developer: TMAH Stepper==
[[Image:SUSS_DEV.JPG|300x300px|right|thumb|The Developer-TMAH-Stepper is placed in F-3]]
[[Image:SUSS_DEV.JPG|400px|right|thumb|The Developer-TMAH-Stepper is placed in F-3.]]


This developer is dedicated for development of DUV resists. The developer is fully automatic and can run up to 25 substrates in a batch  4", 6", and 8" size (8" requires tool change). The machine is equipped with 1 developer line, in our case 2,38% TMAH in water (AZ 726 MIF), 1 topside rinse line with water, 1 backside rinse line with water and 1 N2 line for drying.  
This developer is dedicated for development of DUV resists. The developer is fully automatic and can run up to 25 substrates in a batch  4", 6", and 8" size (8" requires tool change). The machine is equipped with 1 developer line, in our case 2,38% TMAH in water (AZ 726 MIF), 1 topside rinse line with water, 1 backside rinse line with water and 1 N2 line for drying.