Specific Process Knowledge/Thermal Process/RTP Annealsys: Difference between revisions
Appearance
Tag: Manual revert |
|||
| Line 8: | Line 8: | ||
==The Set-Up== | ==The Set-Up== | ||
[[File:Set up.png|650px|thumb|right|Schematic representation of the rapid thermal processor set-up profile view. The substrate (in green) rests on top of three quartz pins, supported by a quartz holder (in black). The drawing is not to scale. Image: Inês Diogo@DTU Nanolab]] | |||
The RTP Annealsys system is divided into two main parts: the process chamber and the loadlock. | The RTP Annealsys system is divided into two main parts: the process chamber and the loadlock. | ||
The chamber has stainless steel walls (water-cooled) and a top and bottom halogen lamp-configuration (16 infra-red lamps, in total). As such, the samples are rapidly heated from both sides, simultaneously. In addition, the chamber is enclosed by two quartz-windows (immediately below/above the set of top/bottom lamps) and these are air-cooled. It is also connected to two external vacuum pumps, to a gas inlet and the loadlock. | The chamber has stainless steel walls (water-cooled) and a top and bottom halogen lamp-configuration (16 infra-red lamps, in total). As such, the samples are rapidly heated from both sides, simultaneously. In addition, the chamber is enclosed by two quartz-windows (immediately below/above the set of top/bottom lamps) and these are air-cooled. It is also connected to two external vacuum pumps, to a gas inlet and the loadlock. | ||
Similarly, the loadlock is also connected to two external pumps. Moreover, the chamber and the loadlock are separated by the gate valve. While processing, the valve remains closed; it is only opened to exchange the substrates when both chamber and loadlock are under turbo vacuum. The substrate transfer is possible due to the mechanical, retractable arm. | Similarly, the loadlock is also connected to two external pumps. Moreover, the chamber and the loadlock are separated by the gate valve. While processing, the valve remains closed; it is only opened to exchange the substrates when both chamber and loadlock are under turbo vacuum. The substrate transfer is possible due to the mechanical, retractable arm. | ||