Specific Process Knowledge/Lithography/Resist/DUVresist: Difference between revisions

From LabAdviser
Jehem (talk | contribs)
Jehem (talk | contribs)
Line 2: Line 2:
The spinning process will be performed by the customer together with the Photolith group of Nanolab. In case you would like to do DUV lithography please contact Lithography team, who will consult you and run your wafers together with you.  
The spinning process will be performed by the customer together with the Photolith group of Nanolab. In case you would like to do DUV lithography please contact Lithography team, who will consult you and run your wafers together with you.  


Information about resist can be found here:


*Bottom Anti Reflection Coating (BARC) [http://www.brewerscience.com/products/arc/dry-etch-arc-coatings/248nm-products/duv42s DUV 42S-6] [[Media:Datasheet_DUV42S.pdf |Datasheet DUV42S-6]].
'''Bottom Anti Reflection Coating (BARC):'''
*Positive DUV resist for spin coating in 600-300nm thickness range [[Media:M230Y_PSM_annular_130C_PEB.pdf|KRF M230Y]].
*Manufacturers website: [http://www.brewerscience.com/products/arc/dry-etch-arc-coatings/248nm-products/duv42s DUV 42S-6]
*Positive DUV resist for spin coating in 1600-800nm thickness range [[Media:M35G_Danchip_intro.pdf|KRF M35G]].
*Datasheet: [https://labmanager.dtu.dk/view_binary.php?class=MiscDocument&id=4&name=Datasheet+DUV42S.pdf DUV42S-6] - '''requires login'''
*Negative DUV resist for spin coating in 1400-800nm or diluted with EC Solvent in 1:1 in 400-200nm thickness range [[Media:UVN2300.pdf|UVN2300-0.8]].
 
 
'''Positive DUV resist for spin coating in 600-300nm thickness range:'''
*[[Media:M230Y_PSM_annular_130C_PEB.pdf|KRF M230Y]]
 
 
'''Positive DUV resist for spin coating in 1600-800nm thickness range:'''
*[[Media:M35G_Danchip_intro.pdf|KRF M35G]]
 
 
'''Negative DUV resist for spin coating in 1400-800nm or diluted with EC Solvent in 1:1 in 400-200nm thickness range:'''
*[[Media:UVN2300.pdf|UVN2300-0.8]].

Revision as of 12:48, 2 February 2023

DUV resist overview

The spinning process will be performed by the customer together with the Photolith group of Nanolab. In case you would like to do DUV lithography please contact Lithography team, who will consult you and run your wafers together with you.


Bottom Anti Reflection Coating (BARC):


Positive DUV resist for spin coating in 600-300nm thickness range:


Positive DUV resist for spin coating in 1600-800nm thickness range:


Negative DUV resist for spin coating in 1400-800nm or diluted with EC Solvent in 1:1 in 400-200nm thickness range: