| Line 81: | Line 81: | ||
[[File:nH E-time.png|500px|left|thumb|'''''Nanoholes profile when varying the ramping E-time .''''']] | [[File:nH E-time.png|500px|left|thumb|'''''Nanoholes profile when varying the ramping E-time .''''']] | ||
{| border="1" style="text-align: center; width: 650px; height: 200px" | {| border="1" style="text-align: center; width: 650px; height: 200px" | ||
|+ 200nm nanoholes recipe from | |+ 200nm nanoholes recipe from July 2022 | ||
|- | |- | ||