Jump to content

Specific Process Knowledge/Thermal Process/RTP Annealsys: Difference between revisions

From LabAdviser
Indiogo (talk | contribs)
Indiogo (talk | contribs)
Line 12: Line 12:
RTP Annealsys offers an optical pyrometry system for temperature measurement, not requiring any contact with the wafer.
RTP Annealsys offers an optical pyrometry system for temperature measurement, not requiring any contact with the wafer.


Regarding controlling the temperature during our process, it is also important to mention the tool can function under two distinct modes – power and temperature control modes. In other words, using power control mode, the tool is programmed to fix the lamp’s power at a specific value (%) and consequently, the temperature inside the chamber varies with time; using the temperature control mode, the tool is programmed to vary the lamps’ power to maintain the temperature stable and constant inside the chamber at a previously established value in the recipe.
Regarding setting the process temperature, it is also important to mention the tool can function under two distinct modes – power and temperature/pyro control modes. In other words, using power control mode, the tool is programmed to fix the lamp’s power at a specific value (%) and consequently, the temperature inside the chamber varies with time; using the temperature/pyro control mode, the tool is programmed to vary the lamps’ power to maintain the temperature stable and constant inside the chamber at a previously established value in the recipe.


'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20https://labadviser.nanolab.dtu.dk/index.php?title=Specific_Process_Knowledge/Thermal_Process/RTP_Annealsys click here]'''
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20https://labadviser.nanolab.dtu.dk/index.php?title=Specific_Process_Knowledge/Thermal_Process/RTP_Annealsys click here]'''

Revision as of 17:04, 24 January 2023

THIS PAGE IS UNDER CONSTRUCTION

RTP Annealsys - Rapid Thermal Processor

January 2023: The RTP Annealsys is being tested, but it is not released for general use yet. Please contact thinfilm@nanolab.dtu.dk for more information.

RTP Annealsys (RTP AS-Premium, serial number AS0415C4 - 7484, from ANNEALSYS) is a research tool available at DTU Nanolab that can reach very high temperatures in a matter of a few minutes or even seconds. Therefore, it is able to perform several types of rapid thermal processing and it can be used as a multi-functional and versatile microfabrication tool, within specific process windows for each process type, using Si/nanofabricated Si structures. Currently, it is used for rapid thermal annealing and smoothing of silicon substrates.

The Set-Up

The chamber in RTP Annealsys possesses a top and bottom halogen lamp-configuration (16 infra-red lamps). As such, the samples are rapidly heated from both sides, simultaneously. In addition, the chamber is enclosed by two quartz-windows (immediately below/above the set of top/bottom lamps) and it is connected to two external vacuum pumps, to a gas inlet and the loadlock. Similarly, the loadlock is also connected to two external pumps. Moreover, the chamber and the loadlock are separated by the gate valve. While processing, the valve remains closed; it is only opened to exchange the substrates when both chamber and loadlock are under vacuum. The substrate transfer is possible due to the mechanical, retractable arm.

Temperature Measurement and Control

RTP Annealsys offers an optical pyrometry system for temperature measurement, not requiring any contact with the wafer.

Regarding setting the process temperature, it is also important to mention the tool can function under two distinct modes – power and temperature/pyro control modes. In other words, using power control mode, the tool is programmed to fix the lamp’s power at a specific value (%) and consequently, the temperature inside the chamber varies with time; using the temperature/pyro control mode, the tool is programmed to vary the lamps’ power to maintain the temperature stable and constant inside the chamber at a previously established value in the recipe.

Feedback to this page: click here