Specific Process Knowledge/Etch/DRIE-Pegasus/Pegasus-2/ORE with Al2O3 mask: Difference between revisions
| Line 37: | Line 37: | ||
=== Holes === | === Holes === | ||
Using patterned samples of 1 μm holes with 50 nm of Al<sub>2</sub>O<sub>3</sub>. After the tests, approximately 20nm of Al<sub>2</sub>O<sub>3</sub> were still intact. | |||
{| border="1" style="text-align: center; width: 900px; height: 200px" | {| border="1" style="text-align: center; width: 900px; height: 200px" | ||
Revision as of 11:44, 19 January 2023
Feedback to this page: click here
THIS PAGE IS UNDER CONSTRUCTION
By Maria Farinha @nanolab, Jan 2023
Important! The pressure settings used below may no longer be permitted, always check with the Dry etch group.
As stated by Nguyen et al., the SF6 and O2 fluxes are only separated after 4 s during the C-step. Shorter time steps than that do not execute the function of the clearing. After testing recipes with only 2 s of clearing and with no clear step, it was understood it could be eliminated, showing more depth as well as less undercut when going for shorter cycles. From then on, not CORE but ORE recipes were applied D/E = O/RE.
Moreover, during the E-step, the MFC (mass flow controller) presented a delay to read the pressure when compared with the power, creating unwanted bias. To fight it, the E-step was divided into E1 and E2. The E1 of only 2 s is enough to stabilize the pressure, and E2 the profile is etch correctly, without the unwanted bias.

Pillars
Using patterned samples of 1 μm pillars with 50 nm of Al2O3. After the tests, approximately 20nm of Al2O3 were still intact.
* Pillars profile effect when varying the etch time.
Holes
Using patterned samples of 1 μm holes with 50 nm of Al2O3. After the tests, approximately 20nm of Al2O3 were still intact.
* For #288 cycles, 120 min, the profile depth reaches 17.6 μm. For #144 cycles, 60 min, the profile depth reaches 10.1 μm. Width variation presented in the pictures.
Nanoholes
| Time (s) | Pressure (valve control) | O2 flow (SCCM) | SF6 flow (SCCM) | Platen power (W) | |
|---|---|---|---|---|---|
| O-step | |||||
| R-step | |||||
| E1-step | |||||
| E2-step |