Sicicon Carbide (SiC) can be deposited by RF-sputtering method. So far the process has been tested only using [[Specific Process Knowledge/Thin film deposition/Lesker|Sputter-System (Lesker)]]:
Silicon Carbide (SiC) can be deposited by RF-sputtering method. So far the process has been tested only using [[Specific Process Knowledge/Thin film deposition/Lesker|Sputter-System (Lesker)]]:


*[[/Deposition of SiC in Sputter-System Lesker|Deposition of SiC in Sputter-System (Lesker)]]
*[[/Deposition of SiC in Sputter-System Lesker|Deposition of SiC in Sputter-System (Lesker)]]

Revision as of 19:46, 20 December 2022

Feedback to this page: film deposition/Deposition of Silicon Carbide click here


Deposition of Silicon Carbide

Silicon Carbide (SiC) can be deposited by RF-sputtering method. So far the process has been tested only using Sputter-System (Lesker):