Specific Process Knowledge/Etch/DRIE-Pegasus/Pegasus-4/Slow etch: Difference between revisions
Appearance
| Line 62: | Line 62: | ||
<br clear="all" /> | <br clear="all" /> | ||
<gallery> | <gallery caption="Map of etch rate measurements" widths="250px" heights="250px" perrow="2"> | ||
File:contour plot for etchrate of slow etch in SiO2.JPG | File:contour plot for etchrate of slow etch in SiO2.JPG| Etch rate map of SiO2 etch on 6" wafer | ||
File:contour plot for etchrate of slow etch in SRN.JPG | File:contour plot for etchrate of slow etch in SRN.JPG| Etch rate map of SRN etch on 6" wafer | ||
</gallery> | </gallery> | ||