== Tungsten deposition ==
= Tungsten deposition =


Tungsten (W) can be deposited by e-beam evaporation and sputtering. However, in case of evaporation the precess generates a lot of heat (despite water cooling), and this means the pressure rises as the chamber is baking out. It is therefore not easy to deposit films much thicker than 50-60 nm. In the Temescal we stopped the deposition every 20 nm to let the pressure drop. Also, the rate needs to be low, to avoid overheating. Talk to staff when you want to deposit W (write to thinfilm@nanolab.dtu.dk). Sputtering can be used without any sufficient issues. In the chart below you can compare the deposition equipment.
Tungsten (W) can be deposited by e-beam evaporation and sputtering. However, in case of evaporation the precess generates a lot of heat (despite water cooling), and this means the pressure rises as the chamber is baking out. It is therefore not easy to deposit films much thicker than 50-60 nm. In the Temescal we stopped the deposition every 20 nm to let the pressure drop. Also, the rate needs to be low, to avoid overheating. Talk to staff when you want to deposit W (write to thinfilm@nanolab.dtu.dk). Sputtering can be used without any sufficient issues. In the chart below you can compare the deposition equipment.
==Sputtering of W==
*[[/Sputtering of W in Sputter Coater 3|Sputtering of Tungsten in the Sputter Coater 3]]





Revision as of 19:25, 14 December 2022

Feedback to this page: click here

Tungsten deposition

Tungsten (W) can be deposited by e-beam evaporation and sputtering. However, in case of evaporation the precess generates a lot of heat (despite water cooling), and this means the pressure rises as the chamber is baking out. It is therefore not easy to deposit films much thicker than 50-60 nm. In the Temescal we stopped the deposition every 20 nm to let the pressure drop. Also, the rate needs to be low, to avoid overheating. Talk to staff when you want to deposit W (write to thinfilm@nanolab.dtu.dk). Sputtering can be used without any sufficient issues. In the chart below you can compare the deposition equipment.

Sputtering of W



E-beam evaporation (Temescal) Sputter-system (Lesker)
General description E-beam evaporation of W Sputtering of W
Pre-clean Ar ion beam None
Layer thickness 10Å to 50nm* 10Å to 600nm
Deposition rate 0.5 Å/s to 1 Å/s about 1 Å/s
Batch size
  • Up to 4x6" wafers
  • Up to 3x8" wafers (ask for holder)
  • small pieces
  • Up to 1x4" wafers
  • Up to 1x6" wafer
  • small pieces
Allowed materials
  • Silicon
  • Silicon oxide
  • Silicon (oxy)nitride
  • Photoresist
  • PMMA
  • Mylar
  • SU-8
  • Metals
  • Silicon
  • Silicon oxide
  • Silicon (oxy)nitride
  • Photoresist
  • PMMA
  • Mylar
  • SU-8
  • Metals
Comments Substrate gets hot during deposition

(for a 60 nm film it rose above 123 C)

Deposition rate is 0.083 nm/s for 150W and 3mTorr