Jump to content

Specific Process Knowledge/Characterization/XRD/SLSII analysis: Difference between revisions

Reet (talk | contribs)
m RS viewer: correcting spelling
Reet (talk | contribs)
Line 111: Line 111:
==Texture==
==Texture==


The texture plugin is used for Pole Figure analysis and Orientation distribution functions (ODF). However we do not have a license for ODF. To enable Orientation functions to be calculated 2 or more pole figures are needed. The texture plugin has two types of calculations, a Defocusing project and texture calculation. The defocusing project will not be discussed here, as it is not strictly needed for the texture calculation, however the idea with this is to measure on substrate with random distributed crystals, and substract this from the oriented texture data.
The texture plugin is used for Pole Figure analysis and Orientation distribution functions (ODF). However we do not have a license for ODF. To enable Orientation functions to be calculated 2 or more pole figures are needed. The texture plugin has two types of calculations, a Defocusing project and texture calculation. The defocusing project will not be discussed here, as it is not strictly needed for the texture calculation, however the idea with this is to measure on substrate with randomly distributed crystals and subtract this from the oriented texture data.


A texture calculation processed as follows:
A texture calculation processed as follows:
*Load data:
*Load data:
**Chose one or more pole figure data sets to load.
**Choose one or more pole figure data sets to load.
*Load defocusing project:
*Load defocusing project:
**This is only possible if a randomly oriented sample has been measured.
**This is only possible if a randomly oriented sample has been measured.