Specific Process Knowledge/Thin film deposition/Deposition of Molybdenum: Difference between revisions
Appearance
No edit summary |
|||
| Line 1: | Line 1: | ||
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php?title=Specific_Process_Knowledge/Thin_film_deposition/Deposition_of_Molybdenum click here]''' | '''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php?title=Specific_Process_Knowledge/Thin_film_deposition/Deposition_of_Molybdenum click here]''' | ||
<i> Unless otherwise stated, this page is written by <b>DTU Nanolab internal</b></i> | |||
== Molybdenum deposition == | == Molybdenum deposition == | ||
Revision as of 17:03, 1 February 2023
Feedback to this page: click here
Unless otherwise stated, this page is written by DTU Nanolab internal
Molybdenum deposition
Molybdenum can be deposited by e-beam evaporation or sputtering. In the chart below you can compare the different deposition equipment.
| E-beam evaporation (Temescal) | Sputter deposition (Lesker) | |
|---|---|---|
| General description | E-beam deposition of Mo
(line-of-sight deposition) |
Sputter deposition of Mo
(not line-of-sight) |
| Pre-clean | Ar ion source | RF Ar clean |
| Layer thickness | 10Å to 0.2 µm* | 10Å to 500 Å |
| Deposition rate | 1Å/s to 10Å/s | Depends on process parameters, roughly about 1 Å/s |
| Batch size |
|
|
| Allowed materials |
|
|
| Comment | As of August 2022, Mo has not yet been deposited in the Temescal.
Please contact the Thin Film group to develop a process. |
* Depending on the amount of heating during Mo deposition, which we will discover during process development.