AR 600-545 and ZED N-50 developers are available in a semi automatic puddle developer '''[[Specific_Process_Knowledge/Lithography/Development#Developer:_E-beam|Developer E-beam]]''' in E-4. It has automatic recipes for puddle development cycles for 10, 30 and 60 seconds of either of the two developers, each finishing off with an IPA rinse and drying cycle.
AR 600-546 and ZED N-50 developers are available in a semi automatic puddle developer '''[[Specific_Process_Knowledge/Lithography/Development#Developer:_E-beam|Developer E-beam]]''' in E-4, mainly intended for development of AR-P 6200 and ZEP 520A. It has automatic recipes for puddle development cycles for 10, 30 and 60 seconds of either of the two developers, each finishing off with an IPA rinse and drying cycle.