Specific Process Knowledge/Etch/ICP Metal Etcher/silicon: Difference between revisions
Appearance
No edit summary |
No edit summary |
||
| Line 4: | Line 4: | ||
== Silicon etching on the ICP Metal Etcher == | == Silicon etching on the ICP Metal Etcher == | ||
<!--Page reviewed by jmli 2/2-2023 --> | |||
{{Template:Author-jmli1}} | |||
In the primary silicon etcher at Nanolab, the [[Specific Process Knowledge/Etch/DRIE-Pegasus|DRIE-Pegasus]], silicon is etched using a fluorine based plasma (with SF<sub>6</sub> as etch gas). Silicon is also etched by chlorine and bromine. | In the primary silicon etcher at Nanolab, the [[Specific Process Knowledge/Etch/DRIE-Pegasus|DRIE-Pegasus]], silicon is etched using a fluorine based plasma (with SF<sub>6</sub> as etch gas). Silicon is also etched by chlorine and bromine. | ||
Revision as of 16:38, 2 February 2023
Feedback to this page: click here
Silicon etching on the ICP Metal Etcher
Unless otherwise stated, all content on this page was created by Jonas Michael-Lindhard, DTU Nanolab
In the primary silicon etcher at Nanolab, the DRIE-Pegasus, silicon is etched using a fluorine based plasma (with SF6 as etch gas). Silicon is also etched by chlorine and bromine.