==Writing fields==
==Writing fields==
Aspects of WF, dimension and resolution, step size
Writefield dimension is a trade off between beam shot precision and field stitching. The maximum writefield size is 1000x1000 µm. The beam controller has a limit of 50000 addressable positions along each axis and hence for a 1000x1000 µm writefield the minimum beam pitch is 20 nm. For a 100x100 µm writefield the minimum beam pitch is 2 nm. Thus the precision is higher for smaller writing fields. Smaller writing fields will however fracture a design into more fields and create more field boundaries with higher potential for stitching errors.