Jump to content

Specific Process Knowledge/Lithography/EBeamLithography/eLINE: Difference between revisions

From LabAdviser
Thope (talk | contribs)
Thope (talk | contribs)
Line 5: Line 5:


==Dose information==  
==Dose information==  
The eLINE tool operates with four different dose types; area dose [pC/cm2], curved element dose [pC/cm2], line dose [pC/cm] and dot dose [pC]. Notice that the last two first are dose per area, while the last two are dose per length and dose per dot, respectively.  
The eLINE tool operates with four different dose types; area dose [µC/cm2], curved element dose [µC/cm2], line dose [pC/cm] and dot dose [pC]. Notice how the units are different for the line and dot doses. Also notice that the unit prefix changes from micro to pico.  


[[File:eLINE-Areas.png]]
[[File:eLINE-Areas.png]]

Revision as of 23:52, 14 June 2022

THIS PAGE IS UNDER CONSTRUCTION

Process information for the Raith eLINE Plus system

The system was installed in the cleanroom in May 2022. As we get more familiar with the tool this page will be populated with relevant process information.

Dose information

The eLINE tool operates with four different dose types; area dose [µC/cm2], curved element dose [µC/cm2], line dose [pC/cm] and dot dose [pC]. Notice how the units are different for the line and dot doses. Also notice that the unit prefix changes from micro to pico.

Table of dose to clear on Si substrate:

Dose [µC/cm2]
Acc. voltage AR-P 6200.09 (180 nm) PMMA 950k AR-N 8200.xx
10 kV 30
20 kV 70
30 kV 100