Line 127: Line 127:
#8                            Cassette from auto stocker shelf 8 is used
#8                            Cassette from auto stocker shelf 8 is used
%4A                          4" wafer in position A is exposed
%4A                          4" wafer in position A is exposed
JDF    'myfirstebl',1         Layer block no. 1 of the jdf-file 'myfirstebl.jdf' is exposed     
JDF    'myfirstebl',1       Layer block no. 1 of the jdf-file 'myfirstebl.jdf' is exposed     
ACC 100                      Acceleration voltage of 100keV is used (can not be changed)
ACC 100                      Acceleration voltage of 100keV is used (can not be changed)
CALPRM '6na_ap5'            The condition file 6na_ap5 is used, i.e. exposure at 6 nA  
CALPRM '6na_ap5'            The condition file 6na_ap5 is used, i.e. exposure at 6 nA