Jump to content

Specific Process Knowledge/Lithography/EBeamLithography/FirstEBL: Difference between revisions

From LabAdviser
Thope (talk | contribs)
Created page with "Under construction, step by step guide to a users first EBL process ===My First E-Beam Lithography Process==="
 
Thope (talk | contribs)
Line 2: Line 2:


===My First E-Beam Lithography Process===
===My First E-Beam Lithography Process===
E-beam lithography and the JEOL 9500 exposure system can be a bit challenging to learn. To help new users along we have set up this page as a step by step guide to your first exposure on the JEOL 9500. For this purpose we will setup a dose test job as an example. This job is fairly simple but it should cover the needs of most users for their first exposure. We strongly encourage users to make sure their first job follows this guide and matches the job defined in this guide in complexity level.
The job set up in this guide will go through the following steps
*Spin coating of e-beam resist
*Job file preparation
*Pattern preparation
*Exposure
*Development

Revision as of 12:24, 26 March 2022

Under construction, step by step guide to a users first EBL process

My First E-Beam Lithography Process

E-beam lithography and the JEOL 9500 exposure system can be a bit challenging to learn. To help new users along we have set up this page as a step by step guide to your first exposure on the JEOL 9500. For this purpose we will setup a dose test job as an example. This job is fairly simple but it should cover the needs of most users for their first exposure. We strongly encourage users to make sure their first job follows this guide and matches the job defined in this guide in complexity level.

The job set up in this guide will go through the following steps

  • Spin coating of e-beam resist
  • Job file preparation
  • Pattern preparation
  • Exposure
  • Development