Created page with "== AR-N 8200 == AR-N 8200 is a negative E-beam resist from All Resist. It is also known as "Medusa 82"." |
No edit summary |
||
| Line 1: | Line 1: | ||
== AR-N 8200 == | == AR-N 8200 == | ||
AR-N 8200 is a negative E-beam resist from | AR-N 8200 is a negative E-beam resist from Allresist, it is also known as "Medusa 82". It is currently (Februrary 2022) being tested at DTU Nanolab. | ||
Revision as of 22:05, 24 February 2022
AR-N 8200
AR-N 8200 is a negative E-beam resist from Allresist, it is also known as "Medusa 82". It is currently (Februrary 2022) being tested at DTU Nanolab.