Eves (talk | contribs)
Created page with "=MgO Sputtering= This page presents the results of MgO deposition using <b>RF sputtering</b> in Sputter-System Lesker, now commonly known as "Old Lesker". The deposition targ..."
 
Eves (talk | contribs)
No edit summary
Line 1: Line 1:
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Thin_film_deposition/Deposition_of_MgO click here]'''
=MgO Sputtering=
=MgO Sputtering=