= How to export data generated by Avantage to CasaXPS = | = How to export data generated by Avantage to CasaXPS = | ||
CasaXPS cannot read the *.vgd files that are generated by Avantage when a spectrum is recorded. All data from Avantage that you wish to analyze using CasaXPS must therefore be manually exported from Avantage. Below is a procedure on how to do this. | CasaXPS cannot read the *.vgd files that are generated by Avantage when a spectrum is recorded. All data from Avantage that you wish to analyze using CasaXPS must therefore be manually exported from Avantage. Below is a procedure on how to do this. | ||