Palladium can be deposited by e-beam evaporation. In the chart below you can compare the different deposition equipment:
| E-beam evaporation (Temescal) | E-beam evaporation (Wordentec) | |
|---|---|---|
| General description | E-beam deposition of Pd | E-beam deposition of Pd |
| Pre-clean | Ar ion source | none |
| Layer thickness | 10 Å - 600 nm* | 10 Å - 600 nm* |
| Deposition rate | 0.5 Å/s to 10Å/s | 2 Å/s to 10Å/s |
| Batch size |
|
|
| Allowed materials |
|
|
| Comment |
* If depositing more than 600 nm, please write to metal@nanolab.dtu.dk well in advance to ensure that enough material is present.