Created page with "Set dose calibration for OneView" |
mNo edit summary |
||
| Line 1: | Line 1: | ||
[[LabAdviser/314/Microscopy 314-307/TEM/ETEM/dose-calibration|Set dose calibration for OneView]] | [[LabAdviser/314/Microscopy 314-307/TEM/ETEM/dose-calibration|Set dose calibration for OneView]] | ||
'''Set dose calibration for OneView camera in Digital Micrograph''' | |||
Here are a few information on the OneView camera and the control in GMS3: | |||
1. Go to "Customs" and "SetDoseCalibrationTag_OneView_mod-DTU" <br /> | |||
[[File:Oneview_1.png|600px|center|thumb|Run script]] | |||
<br clear="all" /> | |||
2. Type in the high tension the microscope is running in the pop-up window<br /> | |||
[[File:Oneview_2.png|300px|center|thumb|Select high tension]] | |||
<br clear="all" /> | |||
3. Don't change the conversion factor; just click on "OK"<br /> | |||
[[File:Oneview_3.png|300px|center|thumb|Don't change conversion factor]] | |||
<br clear="all" /> | |||