Jump to content

Specific Process Knowledge/Etch/ICP Metal Etcher/silicon/isotropic: Difference between revisions

From LabAdviser
Jmli (talk | contribs)
No edit summary
Jmli (talk | contribs)
No edit summary
 
Line 2: Line 2:
<!--Checked for updates on 11/2-2019 - ok/jmli -->
<!--Checked for updates on 11/2-2019 - ok/jmli -->
<!--Checked for updates on 24/8-2021. ok/ jmli-->
<!--Checked for updates on 24/8-2021. ok/ jmli-->
<!--Checked for updates on 4/4-2025 - ok/jmli -->


{| border="1" cellpadding="0" cellspacing="0" style="text-align:center;"
{| border="1" cellpadding="0" cellspacing="0" style="text-align:center;"

Latest revision as of 07:34, 4 April 2025

Isotropic etching in silicon on the ICP Metal Etch

Process parameters
Recipe Step Temp. Time Pres. Hardware Gasses RF powers Observations
SF6 O2 C4F8 Ar CF4 H2 CH4 BCl3 Cl2 HBr Coil Platen SEM images of different runs Keywords
isoslow1 A 20 - 10 - 90 0 0 0 0 0 0 0 0 0 400 3 Click HERE! Note: Lior Shiv got very high etch rate for this recipe >1.5µm/min 2019-07-12
no name, tested by Lior Shiv@Capres 2019-07-12 A 20 - 10 - 90 0 0 0 0 0 0 0 0 0 150 3 About 10% load, etch rate around 400nm/min