|ItemConfiguration= Users and supervisors of Pegasus-2 should carefully read the 3 papers listed in the comments in order to have a correct understanding of the etch process and experimental procedure and how it relates to the Bosch etch performance. | |ItemConfiguration= Users and supervisors of Pegasus-2 should carefully read the 3 papers listed in the comments in order to have a correct understanding of the etch process and experimental procedure and how it relates to the Bosch etch performance. | ||
|ItemComment= | |ItemComment= | ||
*[[media:Black silicon on demand.pdf | On the formation of black silicon in SF6-O2 plasma: The clear, oxidize, remove, and etch (CORE) sequence and black silicon on demand]] | *[[media:Black silicon on demand.pdf | On the formation of black silicon in SF6-O2 plasma: The clear, oxidize, remove, and etch (CORE) sequence and black silicon on demand]] | ||
*[[media:The CORE sequence.pdf | The CORE Sequence: A Nanoscale Fluorocarbon-Free Silicon Plasma Etch Process Based on SF<sub>6</sub>/O<sub>2</sub> Cycles with Excellent 3D Profile Control at Room Temperature ]] | *[[media:The CORE sequence.pdf | The CORE Sequence: A Nanoscale Fluorocarbon-Free Silicon Plasma Etch Process Based on SF<sub>6</sub>/O<sub>2</sub> Cycles with Excellent 3D Profile Control at Room Temperature ]] | ||