Specific Process Knowledge/Thermal Process/RTP Jipelec 2: Difference between revisions
| Line 46: | Line 46: | ||
|style="background:LightGrey; color:black"|Process Temperature | |style="background:LightGrey; color:black"|Process Temperature | ||
|style="background:WhiteSmoke; color:black"| | |style="background:WhiteSmoke; color:black"| | ||
*0- | *0-1200 <sup>o</sup>C | ||
*III-V materials | **Time limits at temperatures above 700 <sup>o</sup>C: | ||
*Temperature ramp | ***700 °C: 60 minutes | ||
***800 °C: 30 minutes | |||
***900 °C: 20 minutes | |||
***1000 °C: 10 minutes | |||
***1100 °C: 5 minutes | |||
***1200 °C: 1 minute | |||
*III-V materials to 450 <sup>o</sup>C | |||
*Temperature ramp: | |||
**Up to 50 <sup>o</sup>C/min with susceptor | |||
**Up to 100 <sup>o</sup>C/min without susceptor | |||
|- | |- | ||
| Line 64: | Line 73: | ||
|style="background:LightGrey; color:black"|Batch size | |style="background:LightGrey; color:black"|Batch size | ||
|style="background:WhiteSmoke; color:black"| | |style="background:WhiteSmoke; color:black"| | ||
* | *200 mm wafers | ||
*Small samples | *150 mm wafers | ||
*100 mm wafers | |||
*50 mm wafers | |||
*Small samples | |||
|- | |- | ||
| style="background:LightGrey; color:black"|Substrate materials allowed | |style="background:LightGrey; color:black"|Substrate materials allowed | ||
|style="background:WhiteSmoke; color:black"| | |style="background:WhiteSmoke; color:black"| | ||
Revision as of 18:54, 15 January 2021
Feedback to this page: click here
THIS PAGE IS UNDER CONSTRUCTION
Jipelec - Rapid Thermal Processing

Jipelec JetFIRST 200 RTP (Rapid Thermal Processer/Annealer).
The main purpose of the machine is to anneal different samples very rapidly, or the machine can be used for alloying.
The machine consists of a process chamber, in which the annealing is done. Samples are placed on quartz pins, either on a graphite sucseptor or, Si dummy wafer or directly in the chamber in the process chamber.
Samples can be 6", 4" wafers or smaller samples made of different materials. In chamber, ht ehte
The maximum annealing temperature is 1200 C, and the heating is done by infrared lamps. Important: check the temperature limits in the table below.
Annnealings can be done at atmospheric pressure or in vacuum. It is also possible to apply a flow of either nitrogen or argon during the annealing.
In the chamber, sample are placed on quartz pins in the bottom of the chamber. 4" and 6" Si wafers can be placed directly on the quartz pins as show in the next picture, or these can be placed on a graphite susceptor. Smaller wafer and smaller samples can be placed on a Si dummy wafer or a graphite susceptor.
The
The Jipelec is a rapid thermal processing (RTP) oven. It is be used for fast and well-controlled annealing or alloying of samples. It is possible to use either a thermocouple or a pyrometer to control the temperature (of the sample carrier).
The user manual, user APV, technical information and contact information can be found in LabManager:
| Purpose | RTP annealing | |
|---|---|---|
| Process parameter range | Process Temperature |
|
| Process pressure |
| |
| Gases on the system |
| |
| Substrates | Batch size |
|
| Substrate materials allowed |
A carrier is always needed: For III-V materials a carbide carrier is used, and for other samples a silicon carrier wafer with 1 µm oxide is used
|