# Providing some of the front and back end films for the CZTS cell, participation in the characterization of the CZTS films, whereas the actual synthesis of CZTS will mostly be done by other project partners.
# Providing some of the front and back end films for the CZTS cell, participation in the characterization of the CZTS films, whereas the actual synthesis of CZTS will mostly be done by other project partners.
# Developing and characterizing the bottom silicon cell.
# Developing and characterizing the bottom silicon cell.
# Developing technology for tunnel/barrier layers on the silicon cell. The purpose of these layers are twofold: 1) At the interface electron currents from the silicon cell must be transformed into hole currents in the CZTS cell. 2) The interface must have a diffusion barrier to protect the silicon cell from in-diffusion of metals (particularly Cu) from the CZTS. This is a particularly challenging task.
# Developing technology for tunnel/barrier layers on the silicon cell. The purpose of these layers are twofold: *1) At the interface electron currents from the silicon cell must be transformed into hole currents in the CZTS cell. *2) The interface must have a diffusion barrier to protect the silicon cell from in-diffusion of metals (particularly Cu) from the CZTS. This is a particularly challenging task.


==Project description==
==Project description==