'''The OES hardware:'''<br>
'''The OES hardware:'''<br>
On a viewport preferably directly facing the plasma above the wafer is chosen. Here, a lens is mounted to focus the emitted light onto an optical fiber feeding it to a spectrometer. The Verity spectrograph has a 200 nm to 800 nm range with a 0.5 nm step.
On a viewport preferably directly facing the plasma above the wafer is chosen. Here, a lens is mounted to focus the emitted light onto an optical fiber feeding it to a spectrometer. The Verity spectrograph and SD1024 controller with SpectraView software are installed on the tools in the list above. It has a 200 nm to 800 nm range with a 0.5 nm step.


'''SpectraView:'''<br>
== Process considerations ==


'''The intensity of the light:'''<br>
'''The intensity of the light:'''<br>