Specific Process Knowledge/Characterization/XPS/XPS Chemical states: Difference between revisions
No edit summary |
No edit summary |
||
| Line 1: | Line 1: | ||
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/ | '''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/ | ||
Characterization/XPS/XPS Chemical states | Characterization/XPS/XPS Chemical states click here]''' | ||
<!--Checked for updates on 2/10-2020 - ok/jmli --> | <!--Checked for updates on 2/10-2020 - ok/jmli --> | ||
Revision as of 15:20, 2 October 2020
Feedback to this page: [mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/ Characterization/XPS/XPS Chemical states click here]
Chemical state
From basic chemistry we know that the chemical properties of an element is determined by the outermost electronic shells. When a chemical bond between two atoms is formed there is an exchange of loosely bonded electrons between them. This exchange of valence electrons induces a small energy shift in all electronic shells of the atoms that may be detected by XPS. This is called the chemical shift. Hence, one can see if, for instance, silicon is in oxidation state 0 (Si-Si bond in bulk silicon) or oxidation state +IV (Four Si-0 bonds in SiO2) by looking at the binding energy of the core level electrons.
The figure to the left illustrates the chemical shift. Si2p XPS spectra were recorded an a Si reference sample and a Si sample that was treated in HF prior to the measurement - and the spectra are clearly different. The spectrum of untreated Si has a clear feature at about 103 eV due to Si atoms bonded to oxygen in the native oxide. In the spectrum from the HF treated sample, only the feature arising from Si-Si interaction is present. Note that both curves only shows the Si signal, but with an clear indication of the chemical state of the Si atoms in the samples.
If you study polymers, you can detect the presence of different chemical groups, for example (C-C),(C-OH),(C=O),(CF3) or (CF2-CH2) in the polymeric layer. And after surface treatments, you may examine differences in the polymeric layer.
Note that binding energies for different chemical states often can be found in the literature.