<gallery caption="" widths="400px" heights="300px" percol="2"> | <gallery caption="" widths="400px" heights="300px" percol="2"> | ||
[[File:BSi free.png|400px|center|thumb|''''' 1 µm silicon pillars etched with a BSi-free recipe''''']] | |||
[[File:BSi full.png|400px|center|thumb|''''' 1 µm silicon pillars etched first with a BSi-free recipe and then continued with a BSi-full recipe''''']] | |||
</gallery> | </gallery> | ||