Silicon wafers are prepared with 1.5 μm thick resist patterns (AZ MIR 701 DUV resist from MicroChemicals) and exposed using a maskless aligner (MLA150, Heidelberg) to create patterns above 400 nm. Below are some SEM images of BSi nanostructures achieved by the modified CORE process:
Silicon wafers are prepared with 1.5 μm thick resist patterns (AZ MIR 701 DUV resist from MicroChemicals) and exposed using a maskless aligner (MLA150, Heidelberg) to create patterns above 400 nm. Below are some SEM images of BSi nanostructures achieved by the modified CORE process:


<gallery caption="" widths="" heights="" perrow="2">
<gallery caption="" perrow="2">
[[File:BSi free.png|400px|center|thumb|''''' 1 µm silicon pillars etched with a BSi-free recipe''''']]
[[File:BSi free.png|400px|center|thumb|''''' 1 µm silicon pillars etched with a BSi-free recipe''''']]